Cellulose 300 Prep TLC Plates

Native Fibrous Cellulose Layers for TLC

  • Fiber length (95%) 2-20µm
  • The average degree of polymerization 400-500
  • Specific surface area according to Blaine 15,000 cm2/g
  • < 20 ppm Fe, 6 ppm Cu, 7 ppm P
  • CH2Cl2 extract = 0.25 %
  • Residue on ignition at 850°C = 1500 ppm

Recommended Applications:

  • Partition chromatography of polar substances such as amino acids, carboxylic acids or carbohydrates
thin layer chromatography beginners